17-7 Irin Din, Coil, Foil, Waya, AMS 5528 (CONDA), AMS 5529 (COND C), ASTM A693, MIL-S25043

Alaye ọja

ọja Tags

Apejuwe

Iru 17-7PH® ojoriro Hardening Alloy jẹ ologbele-austenitic alagbara, irin eyi ti o jẹ austenitic ni anneal majemu, ṣugbọn martensitic ninu awọn àiya majemu. Iru 17-7PH® pese agbara giga ati lile, awọn ohun-ini rirẹ ti o dara julọ, ipata ipata ti o dara ati ipalọlọ ti o kere ju lori itọju ooru. O ti wa ni irọrun ti a ṣẹda ni ipo annealed, lẹhinna lile si awọn ipele agbara giga nipasẹ awọn itọju igbona ti o rọrun si Awọn ipo RH 950 ati TH 1050. Agbara giga ti Iyatọ ti Ipo CH 900 nfunni ni ọpọlọpọ awọn anfani nibiti ductility opin ati iṣẹ ṣiṣe jẹ iyọọda. Ni ipo itọju ooru rẹ, alloy yii n pese awọn ohun-ini ẹrọ iyasọtọ ni awọn iwọn otutu to 900 °F (482 °C).

N08367 - 1.4529 - Incoloy 926 ifi

KẸMISTRY AGBAYE

Inconel 825 ifi

Erogba: 0.090 max

Manganese: 1.00 max

Silikoni: 1.00 max

Chromium: 16.00- 18.00

Nickel: 6.50-7.75

Aluminiomu: 0.75-1.50

Fọsifọọsi: 0.040 max

Efin: 0.030 max

Irin: iwontunwonsi

ASEJE ARA

Ìwúwo: (Cond. A): 0.282 lbs/ni3 7.80 g/cm3

Itanna Resistivity: (microhm-cm) (gbogbo awọn ipo): 60 °F (20 °C): 80

Imudara Ooru: BTU/hr/ft2/ft/°F (W/m•K)

Ni 300 °F (149 °C): 9.5 (16.5)

Itumọ olùsọdipúpọ ti Imugboroosi Gbona: ni/inl°F (µm/m•K): (Cond. A):

70 -200 °F (21 -93 °C): 8.5 x 10-5 (15.3)

70 -400 °F (21 -204 °C): 9.0 x 10-5 (16.2)

70 -600 °F (21 -315 °C): 9.5 x 10-5 (17.1)

70 -800 °F (21 -427 °C): 9.6 x 1 ìwọ-6 (16.0)

Modulu ti Rirọ: ksi (MPa)

29 x 103 (200 x 103) ninu ẹdọfu

Agbara oofa:

Annealed: ferromagnetic ti ko lagbara

Ooru mu: Lagbara ferromagnetic

Fọọmu

Yiyọ okun

  • 17-7PH Irin alagbara, irin rinhoho
  • 17-7PH Irin alagbara, irin bankanje
  • 17-7PH Irin alagbara, irin tẹẹrẹ

Awọn ọja Waya

  • 17-7PH Irin alagbara Irin apẹrẹ Waya & Profaili Waya
  • 17-7PH Irin alagbara, irin Yika Waya
  • 17-7PH Irin Alapin Waya
  • 17-7PH Alagbara Irin Square Waya
Inconel 825 ifi
Inconel 600 gbona ti yiyi farahan

Iṣẹ ṣiṣe

Ṣiṣe awọn ohun-ini ẹrọ iṣelọpọ Ni iwọn otutu yara

Iwọn Iwọn: <.010 inches

Agbara Fifẹ Gbẹhin: 150 KSI max (1035 MPa max)

Agbara Ikore (0.2% aiṣedeede): 65 KSI max (450 MPa max)

Elongation: Kan si alagbawo Ulbrich Technical Services

Iwọn Iwọn:> .010 inches

Agbara Fifẹ Gbẹhin: 150 KSI max (1035 MPa max)

Agbara Ikore (0.2% aiṣedeede): 55 KSI max (380 MPa max)

Ilọsiwaju: 20% min

Lile: Rb 92 max

Ipo Aṣoju C

Agbara Fifẹ Gbẹhin: 200 KSI min (1380 MPa min)

Agbara Ikore (0.2% aiṣedeede): 175 KSI min (1205 MPa min)

Ilọsiwaju: 1 % min

Lile: Tun 41 min (ète)

ÀFIKÚN IRÚNYÌN:

Kan si alagbawo awọn iṣẹ imọ-ẹrọ Ulbrich ti o ba nilo awọn ibinu miiran ju Ipò C.

ITOJU gbigbona TI 17-7PH IRIN ALAIGBỌ

TH 1050 Aṣoju

Agbara Fifẹ Gbẹhin: 180 KSI min (1240 MPa min)

Agbara Ikore: (0.2% Aiṣedeede) 150 KSI min (1034 MPa min)

Elongation: Kan si alagbawo Ulbrich Technical Services

Lile: Tun 38 min

RH950 Aṣoju

Agbara Fifẹ Gbẹhin: 210 KSI min (1450 MPa min)

Agbara Ikore: (0.2 Aiṣedeede) 190 KSI min (1310 MPa min)

Elongation: Kan si alagbawo Ulbrich Technical Services

Lile: Tun 44 min

CH900 Aṣoju

Agbara Fifẹ Gbẹhin: 240 KSI min (1655 MPa min)

Agbara Ikore: (0.2% aiṣedeede) 230 KSI min (1586 MPa min)

Ilọsiwaju: 1 % min

Lile: Tun 46 min (ète)

ÀFIKÚN Properties

IPÁ RESISTANCE OF 17-7PH irin alagbara

Tọkasi NACE (Ẹgbẹ ti Orilẹ-ede ti Awọn Onimọ-ẹrọ Ibajẹ) fun awọn iṣeduro.