Haynes

Alaye ọja

ọja Tags

Giga otutu Alloy

◆ Haynes-188 ni agbara iwọn otutu ti o ga, ti o dara egboogi-ifoyina ati awọn ohun-ini ipata, ti a lo ni lilo pupọ ni afẹfẹ, petrochemical, ọkọ oju omi ati awọn aaye miiran

Kemikali tiwqn

Ipele

C

Si

Mn

S

P

Cr

Ni

Fe

B

Co

W

La

miiran

ko tobi ju

Haynes-188

0.05 ~ 0.15

0.2~0.5

1.25

0.015

0.02

21-23

20-24

≤3

≤0.015

40-45

13-15

0.03 ~ 0.15

-