IInconel
Giga otutu Alloy
◆Inconel600 (N06600) ni o ni ipata resistance si orisirisi ipata media, o tun ni o ni ti o dara ti nrakò rupture agbara, niyanju fun awọn ṣiṣẹ ayika ni isalẹ 700 ℃. O ti wa ni o kun lo ninu awọn aaye ti isejade ati lilo ti ipata alkali awọn irin, paapa ni awọn agbegbe ibi ti sulfides ti wa ni lilo.
◆Iṣẹ pataki ti Inconel601 (N06601) ni pe o ni ifoyina ifoyina ati resistance carbonization ti o dara nigbati iwọn otutu ba ga bi 1180 ° C. O ti lo ni akọkọ ni awọn ẹya iṣelọpọ itọju ooru, awọn ẹya eto eefi, ati awọn reheaters atẹgun.
◆Inconel625 (N06625Ns336) ṣe afihan ipata ipata ti o dara julọ ni ọpọlọpọ awọn media, ati rirọ annealed kekere-carbon alloy 625 ti wa ni lilo pupọ ni ile-iṣẹ ilana kemikali, nibiti o ti kan si omi okun ati duro ni aapọn ẹrọ giga.
◆Inconel725 ni o ni agbara ipata aapọn ati pe o dara fun awọn ohun elo paipu ati awọn ọkọ oju omi okun.
◆Inconel690 ni o ni egboogi-oxidation ati egboogi-ipata-ini, ati ki o jẹ dara fun petrochemical, Metallurgy, iparun agbara, ati be be lo.
Kemikali tiwqn
Ipele | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | Nb | miiran |
ko tobi ju | ||||||||||||||
Inconel600 | 0.15 | 0.5 | 1 | 0.015 | 0.03 | 14-17 | ipilẹ | 6-10 | - | - | ≤0.5 | - | - | - |
Inconel601 | 0.1 | 0.5 | 1 | 0.015 | 0.03 | 21-25 | ipilẹ | 10-15 | 1:1.7 | - | ≤1 | - | - | - |
Inconel625 | 0.1 | 0.5 | 0.5 | 0.015 | 0.015 | 20-23 | ipilẹ | ≤5 | ≤0.4 | ≤0.4 | - | 8-10 | 3.15-4.15 | Co≤1 |
Inconel725 | 0.03 | 0.2 | 0.35 | 0.01 | 0.015 | 19-22.5 | 55-59 | Duro | 0.35 | 1:1.7 | - | 7-9.5 | 2.75~4 | - |
Inconel690 | 0.05 | 0.5 | 0.5 | 0.015 | 0.03 | 27-31 | ≥58 | 7-11 | - | - | ≤0.5 | - | - | - |
Alloy ini kere
Ipele | alloy ipinle | agbara fifẹ RmN/m㎡ | Agbara Ikore Rp0.2N/m㎡ | Ilọsiwaju Bi% | Brinell líle HB |
Inconel600 | Itọju ojutu | 550 | 240 | - | ≤195 |
Itọju ojutu | 500 | 180 | - | ≤185 | |
Inconel601 | Annealing | 650 | 300 | - | - |
Itọju ojutu | 600 | 240 | - | ≤220 | |
Inconel625 | Itọju ojutu | 760 | 345 | - | ≤220 |
Inconel725 | Itọju ojutu | 790 | 485 | 28 | - |
Inconel690 | Itọju ojutu | 780 | 450 | 25 | - |