Monel
Giga otutu Alloy
◆Monel400 ni o ni o tayọ ipata resistance ni hydrofluoric acid ati fluorine gaasi, ati ki o jẹ dara fun pipe paipu ati falifu ti a lo ninu kemikali ise, epo, atomiki agbara, ati tona idagbasoke.
◆Monel500 ni awọn ohun-ini ẹrọ imọ-ẹrọ ti o dara, agbara giga ati idena ipata to dara. O dara fun awọn ohun mimu ati awọn ẹya igbekale ti a lo ninu ile-iṣẹ kemikali, awọn ọkọ oju omi ati imọ-ẹrọ oju omi.
◆Monel404 jẹ lilo pupọ ni petrochemical, ile-iṣẹ iparun, ati awọn paati ile-iṣẹ gige-eti miiran.
Kemikali tiwqn
Ipele | C | Si | Mn | S | P | Cr | Ni | Mo | Fe | Co | W | Al | Ti | Cu |
ko tobi ju | ||||||||||||||
Owo400 | 0.3 | 0.5 | 2 | 0.024 | - | - | ipilẹ | - | ≤2.5 | - | - | - | - | 28-34 |
Owo500 | 0.18 | 0.5 | 1.5 | 0.01 | - | - | ≥63 | - | ≤2 | - | - | 2.3-3.15 | 0.35 ~ 0.85 | 27-33 |
Owo404 | 0.15 | 0.1 | 0.1 | 0.024 | - | - | 52-57 | - | ≤0.5 | - | - | ≤0.05 | - | Duro |
Alloy ini kere
Ipele | Awọn ipo imọ-ẹrọ | agbara fifẹ RmN/m㎡ | Agbara Ikore Rp0.2N/m㎡ | Ilọsiwaju Bi% | Brinell líle HB |
Owo400 | eke / gbona ti yiyi | 516 | 170 | 35 | - |
Annealed ipinle | 483 | 170 | 35 | - | |
Owo500 | Eda ipinle + ti ogbo | 960 | 686 | 20 | 27 |
ri to ojutu + ti ogbo | 896 | 585 | 20 | 24 | |
Owo404 | Annealed ipinle | 550 | 185 | 36 | - |