Nitronic

Alaye ọja

ọja Tags

Giga otutu Alloy

◆Nitronic50 (S20910/XM-19) jẹ irin alagbara austenitic ti a ni imudara nitrogen, eyiti a lo ni akọkọ ni petrochemical, textile, processing ounje ati awọn ile-iṣẹ omi okun.

◆Nitronic60 (S21800 / Alloy218) ni o ni o tayọ ga-otutu ifoyina resistance ati kekere-otutu ikolu išẹ, ati ki o ti wa ni o kun lo ni munadoko egboogi-yiya ati ibere alloy Afara pinni ati awọn miiran bọtini ise agbese.

Kemikali tiwqn

Ipele

C

Si

Mn

S

P

Cr

Ni

Fe

Mo

Ti

Cu

Nb

N

miiran

ko tobi ju

Nitronic50

0.06

1

4~6

0.03

0.04

20.5-23.5

11.5-13.5

ipilẹ

1.5~3

-

-

0.1 0.3

0.2~0.4

-

Nitronic60

0.1

3.5-4.5

7~9

0.03

0.04

16-18

8~9

ipilẹ

-

-

-

-

0.08 ~ 0.18

-

Alloy ini kere

Ipele

ipinle

agbara fifẹ RmN/m㎡

Agbara Ikore Rp0.2N/m㎡

Ilọsiwaju Bi%

Brinell líle HB

Nitronic50

Itọju ojutu

690

380

35

-

Nitronic60

Itọju ojutu

600

320

35

-