SUPER DUPLEX S32760 / F55 / 1.4501

Alaye ọja

ọja Tags

Apejuwe

1.Pese awọn agbara ti o ga ju mejeeji austenitic ati 22% Cr Duplex Stainless Steels UNS S32760 (F55) jẹ ibamu si ọpọlọpọ awọn ohun elo ni awọn ile-iṣẹ bii Epo & Gaasi, CPI (Awọn ile-iṣẹ iṣelọpọ Kemikali), ati awọn agbegbe omi.

UNS S32760 (F55 / 1.4501) ti wa ni atokọ ni NACE MR 01 75 fun iṣẹ ekan ati nini ifọwọsi ASME fun awọn ohun elo Titẹ.

awọn ipele agbara nipasẹ awọn itọju igbona ti o rọrun si Awọn ipo RH 950 ati TH 1050. Agbara giga ti Iyatọ ti Ipò CH 900 nfunni ni ọpọlọpọ awọn anfani nibiti ductility lopin ati iṣẹ ṣiṣe jẹ iyọọda. Ni ipo itọju ooru rẹ, alloy yii n pese awọn ohun-ini ẹrọ iyasọtọ ni awọn iwọn otutu to 900 °F (482 °C).

4Cr14Ni14W2Mo square ifi

Iwe Data Ohun elo

Alloy Super ile oloke meji S32760
Ohun elo No. 1.4501
Aami EN (kukuru) X2CrNiMoCuWN25-7-4
UNS UNS S32760
Aami iṣẹ ti o forukọsilẹ ASTM A182/ F55

Kemikali tiwqn

C Cr Cu Fe Mo Mn
% ≤% ≤%   % %
ti o pọju 0.030 24<26 0.5 <1.0 Olurannileti 3.0 <4.0 1.0 ti o pọju
N Ni P S Si W
% % % % ≤% %
0.20 <0.30 6.0 <8.0 ti o pọju 0.030 ti o pọju 0.010 ti o pọju 0.010 0.50 <1.0

Pataki Properties

Youngs Modul N / mm2 Ìwọ̀n kg/dm³: Oofa Permeability
199 x 10³ 7.81 g/cm³ 33

O tayọ Resistance to pitting ati crevice / ogbara ipata

Awọn pato

Inconel 718 Ifi

● EN 10088-3 1.4501

● ASTM A473 UNS S32760 Forgings

● ASTM A182 ite F55 UNS S32760 eke Flanges

● ASTM A240 UNS S32760 Iwe ati Awo

● ASTM A479 UNS S32760 Pẹpẹ

● ASTM A276 UNS S32760 Ipò A

● NACE MR 01-75

Ohun elo naa wa pẹlu iwe-ẹri 3.1 kan.

Iwe-ẹri 3.2 wa pẹlu afikun.

Darí Properties

0.2% Ẹri Wahala (N/mm2) [ksi] kere ju 550 550 [79.8]
Gbẹhin Fifẹ Agbara (N/mm2) [ksi] kere 750 [108.8]
Elongation (%) kere 25
Lile (HBN) 270 ti o pọju
Idinku Agbegbe Abala Agbelebu (%) o kere julọ 45
Charpy V-ogbontarigi Ipa ni ibaramu Temp (J) [ft.lb] iṣẹju 80 [59 min]
Charpy V-notch Ipa ni -46°C (J) [ft.lb] 45av, iṣẹju 35 [33av, 25.8 min]